Sintered NdFeB Magnet
Sintered NdFeB Magnet Physical Properties | ||||||||
Grade | Remanence | Rev. Temp.- Coeff. Ng Br | Puwersang Puwersa | Intrinsic Coercive Force | Rev. Temp.- Coeff. Ng Hcj | Max. Produktong Enerhiya | Max. Operating Temperatura | Densidad |
Br (KGs) | Hcb (IKAW) | Hcj (IKAW) | (BH) max. (MGOe) | g/cm³ | ||||
N35 | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥12 | -0.58~-0.78 | 33-36 | 80 ℃ | 7.6 |
N38 | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥12 | -0.58~-0.78 | 36-39 | 80 ℃ | 7.6 |
N40 | 12.5-12.8 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 38-41 | 80 ℃ | 7.6 |
N42 | 12.8-13.2 | -0.11~-0.12 | ≥11.5 | ≥12 | -0.58~-0.78 | 40-43 | 80 ℃ | 7.6 |
N45 | 13.2-13.8 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 43-46 | 80 ℃ | 7.6 |
N48 | 13.8-14.2 | -0.11~-0.12 | ≥11.6 | ≥12 | -0.58~-0.78 | 46-49 | 80 ℃ | 7.6 |
N50 | 14.0-14.5 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 48-51 | 80 ℃ | 7.6 |
N52 | 14.3-14.8 | -0.11~-0.12 | ≥10.0 | ≥12 | -0.58~-0.78 | 50-53 | 80 ℃ | 7.6 |
N33M | 11.3-11.7 | -0.11~-0.12 | ≥10.5 | ≥14 | -0.58~-0.72 | 31-33 | 100 ℃ | 7.6 |
N35M | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥14 | -0.58~-0.72 | 33-36 | 100 ℃ | 7.6 |
N38M | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥14 | -0.58~-0.72 | 36-39 | 100 ℃ | 7.6 |
N40M | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥14 | -0.58~-0.72 | 38-41 | 100 ℃ | 7.6 |
N42M | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥14 | -0.58~-0.72 | 40-43 | 100 ℃ | 7.6 |
N45M | 13.2-13.8 | -0.11~-0.12 | ≥12.5 | ≥14 | -0.58~-0.72 | 43-46 | 100 ℃ | 7.6 |
N48M | 13.6-14.3 | -0.11~-0.12 | ≥12.9 | ≥14 | -0.58~-0.72 | 46-49 | 100 ℃ | 7.6 |
N50M | 14.0-14.5 | -0.11~-0.12 | ≥13.0 | ≥14 | -0.58~-0.72 | 48-51 | 100 ℃ | 7.6 |
N35H | 11.7-12.2 | -0.11~-0.12 | ≥10.9 | ≥17 | -0.58~-0.70 | 33-36 | 120 ℃ | 7.6 |
N38H | 12.2-12.5 | -0.11~-0.12 | ≥11.3 | ≥17 | -0.58~-0.70 | 36-39 | 120 ℃ | 7.6 |
N40H | 12.5-12.8 | -0.11~-0.12 | ≥11.6 | ≥17 | -0.58~-0.70 | 38-41 | 120 ℃ | 7.6 |
N42H | 12.8-13.2 | -0.11~-0.12 | ≥12.0 | ≥17 | -0.58~-0.70 | 40-43 | 120 ℃ | 7.6 |
N45H | 13.2-13.6 | -0.11~-0.12 | ≥12.1 | ≥17 | -0.58~-0.70 | 43-46 | 120 ℃ | 7.6 |
N48H | 13.7-14.3 | -0.11~-0.12 | ≥12.5 | ≥17 | -0.58~-0.70 | 46-49 | 120 ℃ | 7.6 |
N35SH | 11.7-12.2 | -0.11~-0.12 | ≥11.0 | ≥20 | -0.56~-0.70 | 33-36 | 150 ℃ | 7.6 |
N38SH | 12.2-12.5 | -0.11~-0.12 | ≥11.4 | ≥20 | -0.56~-0.70 | 36-39 | 150 ℃ | 7.6 |
N40SH | 12.5-12.8 | -0.11~-0.12 | ≥11.8 | ≥20 | -0.56~-0.70 | 38-41 | 150 ℃ | 7.6 |
N42SH | 12.8-13.2 | -0.11~-0.12 | ≥12.4 | ≥20 | -0.56~-0.70 | 40-43 | 150 ℃ | 7.6 |
N45SH | 13.2-13.8 | -0.11~-0.12 | ≥12.6 | ≥20 | -0.56~-0.70 | 43-46 | 150 ℃ | 7.6 |
N28UH | 10.2-10.8 | -0.11~-0.12 | ≥9.6 | ≥25 | -0.52~-0.70 | 26-29 | 180 ℃ | 7.6 |
N30UH | 10.8-11.3 | -0.11~-0.12 | ≥10.2 | ≥25 | -0.52~-0.70 | 28-31 | 180 ℃ | 7.6 |
N33UH | 11.3-11.7 | -0.11~-0.12 | ≥10.7 | ≥25 | -0.52~-0.70 | 31-34 | 180 ℃ | 7.6 |
N35UH | 11.8-12.2 | -0.11~-0.12 | ≥10.8 | ≥25 | -0.52~-0.70 | 33-36 | 180 ℃ | 7.6 |
N38UH | 12.2-12.5 | -0.11~-0.12 | ≥11.0 | ≥25 | -0.52~-0.70 | 36-39 | 180 ℃ | 7.6 |
N40UH | 12.5-12.8 | -0.11~-0.12 | ≥11.3 | ≥25 | -0.52~-0.70 | 38-41 | 180 ℃ | 7.6 |
N28EH | 10.4-10.9 | -0.105~-0.120 | ≥9.8 | ≥30 | -0.48~-0.70 | 26-29 | 200 ℃ | 7.6 |
N30EH | 10.8-11.3 | -0.105~-0.120 | ≥10.2 | ≥30 | -0.48~-0.70 | 28-31 | 200 ℃ | 7.6 |
N33EH | 11.3-11.7 | -0.105~-0.120 | ≥10.5 | ≥30 | -0.48~-0.70 | 31-34 | 200 ℃ | 7.6 |
N35EH | 11.7-12.2 | -0.105~-0.120 | ≥11.0 | ≥30 | -0.48~-0.70 | 33-36 | 200 ℃ | 7.6 |
N38EH | 12.2-12.5 | -0.105~-0.120 | ≥11.3 | ≥30 | -0.48~-0.70 | 36-39 | 200 ℃ | 7.6 |
N28AH | 10.4-10.9 | -0.105~-0.120 | ≥9.9 | ≥33 | -0.45~-0.70 | 26-29 | 230 ℃ | 7.6 |
N30AH | 10.8-11.3 | -0.105~-0.120 | ≥10.3 | ≥33 | -0.45~-0.70 | 28-31 | 230 ℃ | 7.6 |
N33AH | 11.3-11.7 | -0.105~-0.120 | ≥10.6 | ≥33 | -0.45~-0.70 | 31-34 | 230 ℃ | 7.6 |
Tandaan: · Sa ilalim ng temperatura ng pagtatrabaho na 20 ℃ ± 2 ℃, sa itaas ng mga magnetic parameter at pisikal na katangian ay nasubok, na may hindi maiiwasang pagkawala ng magnetic force na hindi hihigit sa 5%.· Ang pinakamataas na temperatura ng pagtatrabaho ng magnet ay nababago dahil sa ratio ng haba at diameter at mga kadahilanan sa kapaligiran . |
Advantage:
Ang mga katangian ng mga magnet na ito ay higit na nakahihigit sa mga tradisyonal at sila ang kasalukuyang pinakamakapangyarihan sa aplikasyon. Ang taas nila
Ang coercivity at mataas na remanence ay nagpapahintulot sa bagong disenyo at ang posibilidad ng pagtaas ng magnetic field ng aplikasyon kung saan limitado ang espasyo
o kung saan kinakailangan ang isang malakas na magnetic field.
Ang mga magnet ng NdFeB ay lubhang madaling kapitan ng kaagnasan. Samakatuwid ay nangangailangan ng proteksiyon na ibabaw na patong. Ang mga paggamit ng NdFeB magnet ay nakakondisyon
sa pamamagitan ng temperatura sa isang malawak na hanay na tumatakbo mula 80ºC hanggang 230ºC. At gumagana rin ito sa temperatura sa ibaba 0 ℃.
Application:
Ang mga neodymium magnet ay ginagamit bilang iba't ibang uri ng magnetic lens para sa pagtutok, pagpapalihis ng mga sisingilin na particle sa electronics, mga sistema ng preno,
drip, sensor, magnetic system sa rotor at micro motors, at larangan ng agham, medisina (tomography, NMR spectrometers), atbp.
Ngayon, ang mga NdFeB magnet ay ginagamit sa maraming dami sa buong mundo. Ang pagbuo ng materyal na ito ay hindi pa kumpleto; ang remanence
at patuloy na nadaragdagan ang lakas ng puwersa sa larangan. Ang mataas na enerhiya ng NdFeB magnets ay nangangahulugan na ang mga motor at sensor ay maaaring itayo
mas maliit - at ito ay nagpapahiwatig ng pagtaas sa kahusayan sa pagganap. Ang patuloy na mga pagpapabuti ay nagbibigay-daan sa kawili-wiling materyal na ito na patuloy na
nual na ipinakilala sa mga bagong lugar.
Ang lahat ng nakasaad na halaga ay natukoy gamit ang mga karaniwang sample ayon sa IEC 60404-5. Ang mga sumusunod na detalye ay nagsisilbing mga halaga ng sanggunian at
maaaring magkaiba. Para sa karagdagang impormasyon mangyaring makipag-ugnayan sa aming mga inhinyero ng aplikasyon.